PRODUCTS
Chloropropylsilane
3-Chloropropyltrichlorosilane
video
3-Chloropropyltrichlorosilane

3-Chloropropyltrichlorosilane

Product code: EB-201

CAS NO.: 2550-06-3

Molecular Formula: Cl(CH2)3SiCl3

Description: 3-Chloropropyltrichlorosilane is an organosilicon compound with the chemical formula Cl(CH₂)₃SiCl₃ and CAS number 2550-06-3. It appears as a clear liquid ranging from colorless to pale yellow. It is primarily used in the synthesis of silane coupling agents such as KH-550 and Si69, as well as organic silicon intermediates and high-molecular-weight polymers. It is typically prepared by the reaction of trichlorosilane with allyl chloride in the presence of a platinum catalyst.

Products Description

3-Chloropropyltrichlorosilane is an organosilicon compound with the chemical formula Cl(CH₂)₃SiCl₃ and CAS number 2550-06-3. It appears as a clear liquid ranging from colorless to pale yellow. It is primarily used in the synthesis of silane coupling agents such as KH-550 and Si69, as well as organic silicon intermediates and high-molecular-weight polymers. It is typically prepared by the reaction of trichlorosilane with allyl chloride in the presence of a platinum catalyst.

Product Information:

● Name: 3-Chloropropyltrichlorosilane

● Synonyms: 3-Chloropropyltrichlorosilane; (3-Chloropropyl)trichlorosilane; Chloropropyltrichlorosilane; 3-Chloropropyltrichlorosilane; 3-Chloropropyltrichlorosilane; 3-Chloropropyltrichlorosilane, Chloropropyltrichlorosilane

● Equivalent Trade Names: Z-6041 (DowCorning), KBE-403 (ShinEtsu), GF82 (Wacker), GLYEO (EVONIK Degussa)

● Molecular Formula: C₃H₆Cl₄Si

● CAS No.: 2550-06-3

● Molecular Weight: 211.98

● Structural Formula:

3-Chloropropyltrichlorosilane

Physical Properties:

● Boiling Point: 181°C

● Density: 1.35 g/mL at 25°C (lit.)

● Refractive Index: 1.465

● Flash Point: 84°C

● Appearance: Colorless transparent liquid

● Specific Gravity: 1.35

● Solubility: Undergoes vigorous hydrolysis upon contact with water; soluble in low-molecular-weight alcohols, hydrocarbons, ethers, and similar solvents

Applications:

3-Chloropropyltrichlorosilane (Cl(CH₂)₃SiCl₃) is one of the most important intermediates in the production of silane coupling agents. It serves as a key raw material for manufacturing various silane coupling agents, including chloropropyltriethoxy (or trimethoxy) silanes, aminopropyltriethoxy (or trimethoxy) silanes, and bis(triethoxysilylpropyl) tetrasulfide. These products are essential additives in rubber formulations and glass fiber-reinforced composite materials.

Storage:

This product should be stored in a dry, cool, and light-protected indoor environment, away from direct sunlight.

Packaging:

● Plastic drums

● Net weights: 5 kg, 25 kg, 200 kg

Disclaimer:

All product information and technical recommendations provided herein are based on our current experience and level of technical knowledge. We do not assume any legal liability, including infringement of third-party intellectual property rights. No warranties or guarantees, either expressed or implied, are made regarding the properties or performance of this product, especially under legal terms. We reserve the right to make changes to the product information at any time due to technological advancements or further developments. Customers are responsible for conducting thorough testing and evaluation of the product prior to use. The descriptions of product properties contained in this document should be verified independently by customers through qualified personnel. Reference to trade names used by other companies does not constitute endorsement, nor does it imply incompatibility or unsuitability of alternative or similar products.


Send Inquiry