Products Description
3-Chloropropyltrimethoxysilane is an organosilicon compound with the chemical formula C₆H₁₅ClO₃Si and CAS No. 2530-87-2. It appears as a colorless, transparent liquid at room temperature and atmospheric pressure. It is insoluble in water but undergoes slow hydrolysis upon contact. The chlorine atom and methoxy groups in its molecular structure confer high reactivity, enabling it to participate in coupling reactions or serve as an intermediate for synthesizing other functional silanes.
Product Information:
● Name: 3-Chloropropyltrimethoxysilane
● Synonyms: (3-Chloropropyl)trimethoxysilane | 3-Chloropropyltrimethoxysilane | Chloropropyltrimethoxysilane | γ-Chloropropyltrimethoxysilane
●Molecular Formula: C₆H₁₅ClO₃Si
● Molecular Weight: 198.72
● CAS No.: 2530-87-2
● Structural Formula:

Physical Properties:
● Density (25 °C): 1.075 ± 0.005 g/cm³
● Boiling Point: 195–196 °C
● Flash Point: 75 °C
● Appearance: Colorless transparent liquid
● Solubility: Hydrolyzes upon contact with water; soluble in low-molecular-weight alcohols, hydrocarbons, ethers, and similar solvents
Applications:
This product is an intermediate used in the production of silane coupling agents. It can be directly employed as a coupling agent or serve as a raw material for synthesizing other coupling agents.
Storage:
Store in a dry, cool, and light-protected indoor environment.
Packaging:
Plastic drums, net weight: 25 kg, 200 kg.
Disclaimer:
All product information and technical recommendations provided herein are based on our current experience and level of knowledge. We assume no legal liability, including with respect to any third-party intellectual property rights. No warranties or guarantees, either expressed or implied, are made regarding the properties of the product, especially in legal terms. We reserve the right to make changes to the product information at any time due to technological advancements or further developments. Customers are responsible for conducting thorough testing and evaluation of the product on their own. The descriptions of product properties contained in this document should also be verified independently by customers through qualified professionals. Tradenames or references used by other companies are mentioned solely for identification purposes and do not imply recommendation or exclusion of similar, potentially available products.