EB-999 (Hexamethyldisilazane CAS 999-97-3) is a silazane supplied worldwide by Guangzhou Epoxysca Material Technology Co., Ltd. Si-N bonds provide specific reactivity for ceramic precursor and surface-treatment applications. It is available in export-grade packaging: a batch COA is provided with every shipment, and English TDS/MSDS can be requested from our sales team. Sea or air shipment is arranged according to the goods class and destination requirements. Typical applications include specialty applications and specialty applications.

| Chemical Name | Hexamethyldisilazane |
|---|---|
| CAS No. | 999-97-3 |
| EINECS No. | 213-668-5 |
| Molecular Formula / MW | C₆H₁₉NSi₂ / 161.39 |
| Appearance | Colorless transparent liquid |
Applications
- Specialty applications:Improves interface bonding and dispersion in the target system Contact us for the English TDS and sample support.
- Specialty applications:Improves interface bonding and dispersion in the target system Export packing and documents are available for this application.
- Specialty applications:Improves interface bonding and dispersion in the target system Contact us for the English TDS and sample support.
- Specialty applications:Improves interface bonding and dispersion in the target system Export packing and documents are available for this application.
Usage & Recommended Dosage
Common process routes and dosage references for EB-999 are summarized below. Detailed English process instructions are available on request.
Priming: process details are provided in the English TDS — contact our technical team.
Recommended practice: process details are provided in the English TDS — contact our technical team.
Packaging & Storage
Store sealed in a cool, dry and ventilated place, away from light and moisture. Standard packing: 20 kg carton, 25 kg plastic drum, 200 kg steel drum or IBC. Other packings available on request. Shelf life: 12 months in unopened original packaging.
Frequently Asked Questions
Can you supply EB-999 for export?
Yes. EB-999 (silazane) is supplied worldwide from Guangzhou Epoxysca. Sea freight (FCL/LCL) and air freight are both available; packing and documents follow the hazardous-goods class and destination port requirements.
How can I get the English TDS, MSDS and COA of EB-999?
A batch COA is provided with every shipment. English TDS and MSDS can be requested from our sales team when inquiring; the technical data on this page follows the same specification as the COA.
What is the MOQ and lead time for EB-999?
Both sample-size and full-packing orders are acceptable. Regular lead time is confirmed per order; sea and air schedules can be arranged according to your destination port or airport.
What are the main applications of EB-999?
Specialty applications and Specialty applications are the primary applications. For formulation advice and dosage recommendations, please refer to the usage section or contact our technical team.