Products Description
n-Propylmethyldimethoxysilane is an organosilicon compound with the chemical formula C₆H₁₆O₂Si and CAS No. 18173-73-4. It appears as a colorless liquid, with a molecular weight of 148.2755, density of 0.842 g/cm³, boiling point of 120.6°C, and flash point of 9.2°C. Primarily used as a silane coupling agent, n-propylmethyldimethoxysilane improves adhesion between organic and inorganic materials, and finds wide applications in industrial products such as coatings, adhesives, and plastics.
Basic Information:
●
Chemical Name:n-Propylmethyldimethoxysilane
● Synonyms:dimethoxymethylpropyl silane ,Propylmethyldimethoxysilane
● CAS Number: 18173-73-4
● EINECS Number: 225-931-1
Molecular Weight: 148.28
Molecular Formula: C₆H₁₆O₂Si
Chemical Structure:

Physical Properties:
● Density: 0.842 g/cm³
● Boiling Point: 120.6°C
● Flash Point: 9.2°C
● Appearance: Colorless transparent liquid
● Purity: ≥98%
Applications:
n-Propylmethyldimethoxysilane is a difunctional silane with relatively low surface tension. It can be used as a surfactant and as a dispersant in surface treatment and coating applications, enhancing the adhesion and corrosion resistance of coatings. It is also employed in the production of silicone resins and other organosilicon polymers.
Packaging and Storage:
● 20 kg carton containing four 5 kg plastic pails
● 200 kg PVF steel or plastic drums
● 1,000 kg IBC totes
[Disclaimer:]
All product information and technical recommendations provided herein are based on our current experience and level of knowledge. We assume no legal liability, including with regard to any third-party intellectual property rights that may be involved. No warranties or guarantees, either expressed or implied, are made regarding the properties of the product, especially in legal terms. We reserve the right to make any changes to the product information due to technological advancements or further developments. Customers are responsible for conducting thorough testing and evaluation of the product on their own. The descriptions of product properties in this document should be verified by customers through professional testing. References to trade names used by other companies do not constitute recommendations nor imply incompatibility or exclusion of similar products.