PRODUCTS
Aminosilane
Bis-(3-trimethoxysilylpropyl)amine |Crosslinking
video
Bis-(3-trimethoxysilylpropyl)amine |Crosslinking

Bis-(3-trimethoxysilylpropyl)amine |Crosslinking

Product code: A-1170

CAS NO.: 82985-35-1

Molecular Formula: C12H31NO6Si2

Description: ​A-1170 Bis-(3-trimethoxysilylpropyl)amine is a diamino silane coupling agent, chemically known as bis(3-trimethoxysilylpropyl)amine, CAS No. 82985-35-1. It is a low-viscosity, light yellow, clear and transparent liquid with a slight ammoniacal odor and has the molecular formula C12H31NO6Si2. Its unique secondary amine structure provides milder and delayed reactivity, resulting in enhanced stability. A-1170 can serve as a crosslinking agent for amine-terminated or modified resins such as epoxy and polyurethane resins, imparting moisture-curing properties to the polymers.

Products Description

A-1170 Bis-(3-trimethoxysilylpropyl)amine is a diamino silane coupling agent, chemically known as bis(3-trimethoxysilylpropyl)amine, CAS No. 82985-35-1. It is a low-viscosity, light yellow, clear and transparent liquid with a slight ammoniacal odor and has the molecular formula C12H31NO6Si2. Its unique secondary amine structure provides milder and delayed reactivity, resulting in enhanced stability. A-1170 can serve as a crosslinking agent for amine-terminated or modified resins such as epoxy and polyurethane resins, imparting moisture-curing properties to the polymers.

Basic Information:

● Chemical Name: Bis-(3-trimethoxysilylpropyl)amine

● Molecular Formula: C12H31NO6Si2

● Structural Formula:

Bis-(3-trimethoxysilylpropyl)amine |Crosslinking

● Molecular Weight: 341.55

● CAS No.: 82985-35-1

Equivalent International Product Numbers:

● Momentive (USA): A-1170

● Evonik (Germany): Evonik 1124

Physical Properties:

● Appearance: Clear liquid

● Color: Colorless to light yellow

● Purity, %: ≥ 98%

● Specific Gravity (25°C): 1.04

● Boiling Point (°C): 285

● Refractive Index (nD at 25°C): 1.432

● Flash Point (Closed Cup, °C): 110

Key Properties:

● Excellent crosslinking capability

● Improved adhesion to substrates

● Enhanced flexural strength, tensile strength, impact resistance, and elastic modulus

● Improved water resistance and corrosion resistance, with excellent durability under high temperature and high humidity conditions

● Enhanced wetting performance and improved rheological properties

● Better filler dispersion, enabling higher filler loading levels

Applications:

1. Can be used as an adhesion promoter in the coatings and sealants industries.

2. Suitable as a coupling agent in foundry and casting applications to improve mechanical properties.

3. Can function as a surface protector and adhesion promoter in the formulation of metal silanization surface treatment agents.

4. Applicable to thermoplastic resins such as epoxy, polyurethane, phenolic, melamine, polyimide, and furan resins, improving filler compatibility and enhancing resin adhesion to inorganic substrates.

5. As a diamino silane, it can act as a water-based coupling agent, promoting adhesion between different materials and facilitating the formation of hybrid materials.

Handling and Storage:

Store in a sealed container in a cool, well-ventilated, and dry area. Protect from moisture and fire hazards. Packaged in plastic drums, net weight 200 kg per drum. Other packaging specifications can be provided upon request.

Disclaimer:

All product information and technical recommendations provided herein are based on our current experience and level of knowledge. We assume no legal liability, including with regard to any known third-party intellectual property rights. No warranties or guarantees, either expressed or implied, are made regarding the properties of the product, especially in legal terms. We reserve the right to make changes to the product information at any time due to technological advancements or further developments. Customers are responsible for conducting thorough testing and evaluation of the product. Descriptions of product properties included in this document should be independently verified by customers through qualified professionals. Reference to trademarks or product names of other companies does not constitute endorsement, nor does it imply incompatibility or unsuitability of alternative or similar products.