PRODUCTS
Aminosilane
Amino Silane Oligomer
video
Amino Silane Oligomer

Amino Silane Oligomer

Product code: EB1100

CAS NO.:

Molecular Formula:

Description: Product Description:Product Name: Amino Silane OligomerProduct Code: EB1100[Typical Physical Properties]:Density (20°C, g/cm³): 1.0380–1.0480Refractive Index (n²⁰D): 1.4420–1.4520Appearance: Colorless to pale yellow transparent liquidSolubility: Soluble in alcohols; hydrolyza

Products Description

Product Description:

Product Name: Amino Silane Oligomer

Product Code: EB1100

[Typical Physical Properties]:

Density (20°C, g/cm³): 1.0380–1.0480 

Refractive Index (n²⁰D): 1.4420–1.4520 

Appearance: Colorless to pale yellow transparent liquid 

Solubility: Soluble in alcohols; hydrolyzable in water

Applications:

1. Suitable for formulations in aqueous systems. Primarily used as a key additive in waterborne coatings and primers, water-based adhesives, and sealants. It helps reduce system viscosity and improves processability.

2. Used for surface modification of inorganic fillers such as glass fibers, kaolin, precipitated silica, wollastonite, and other powdery materials. Especially suitable for wet surface treatment, enhancing adhesion and mechanical properties in high-performance composite materials.

3. Acts as a bonding enhancer for thermosetting and thermoplastic resins, and as an adhesion promoter for sealants.

4. Can be applied in surface treatment of metals.

Storage and Handling:

Store in a well-ventilated, dry environment. Keep containers tightly sealed to prevent moisture absorption. (Strictly avoid storage with acids, flammable materials, reducing agents, etc.)

Packaging:

Plastic drums, net weight: 25 kg / 200 kg.

Disclaimer:

All product information and technical recommendations provided herein are based on our current experience and knowledge. We assume no legal liability, including with regard to any third-party intellectual property rights already known. No warranties or guarantees, whether expressed or implied, are made regarding the properties of the product, especially in legal terms. We reserve the right to make any changes to the product information due to technological advancements or further developments. Customers are responsible for conducting thorough testing and evaluation of the product on their own. The descriptions of product properties in this document should be verified by customers through testing performed by qualified professionals. Reference designations from other companies mentioned herein are neither recommendations nor do they imply incompatibility or unsuitability of alternative, similar products.