Products Description
N-Phenyl-γ-aminopropyltrimethoxysilane (CAS No.: 3068-76-6) is an organosilicon compound with the chemical formula C₁₂H₂₁NO₃Si and a molecular weight of approximately 255.39. It appears as a clear liquid, ranging from colorless to pale yellow at room temperature. Also known as 3-(Phenylamino)propyltrimethoxysilane or N-Phenyl-3-aminopropyltrimethoxysilane, this compound features an aniline group that confers enhanced stability to the reactivity of the amino function. N-Phenyl-γ-aminopropyltrimethoxysilane is primarily used as an adhesion promoter, bonding aid, and additive, playing a significant role in various composite materials and resin systems.
Basic Information:
● Chemical Name: N-Phenyl-γ-aminopropyltrimethoxysilane
● Molecular Formula: C₁₂H₂₁NO₃Si
● Structural Formula:

● Molecular Weight: 255.39
● CAS No.: 3068-76-6
● EINECS No.: 221-328-2
Equivalent Foreign Brands:
● Momentive: Y-9669
● Dow Corning: SZ-6083
● Shin-Etsu (Japan): KBM-573
Physical Properties:
● Appearance: Clear liquid
● Color: Pale yellow
● Purity (%): ≥ 98%
● Specific Gravity (at 25°C): 1.070
● Boiling Point (°C): 309.60
● Refractive Index (nD at 25°C): 1.505
● Flash Point (Closed Cup, °C): 131.29
Key Properties:
● Material Performance Enhancement: Effectively improves mechanical properties, electrical performance, thermal resistance, weatherability, and adhesion of materials.
● Silanization of Metal Surfaces: Widely applied in the silanization treatment of metal surfaces to enhance corrosion resistance and adhesion.
● Coupling Agent for Glass Coatings: Acts as a coupling agent in glass paints, improving adhesion between glass substrates and coating materials.
● Adhesive and Sealant Industry: Significantly enhances the performance and stability of products used in electronic encapsulants, adhesives, and sealants.
Applications:
1. Serves as a coupling agent to promote adhesion between polyurethane, epoxy, acrylic, and phenolic resins and substrates such as glass, metals, glass fibers, and inorganic fillers.
2. Applied in adhesives, sealants, coatings, sizing agents and surface treatments for glass fibers, primers, and foundry sand binders.
3. Improves the high-temperature aging resistance of glass fiber-reinforced phenolic composites.
Handling and Storage:
Store in a sealed container in a cool, well-ventilated, and dry area. Protect from moisture and fire hazards. Packaged in plastic drums, each net weighing 200 kg. Customized packaging options are also available upon request.
Disclaimer:
All product information and technical suggestions provided herein are based on our current experience and knowledge. We assume no legal liability, including with regard to any third-party intellectual property rights. No warranties or guarantees, either expressed or implied, are made regarding the properties of this product, especially under legal standards. We reserve the right to modify the information contained in this document at any time due to technological advancements or further developments. Customers are responsible for conducting thorough testing and evaluation of the product. The descriptions of product properties should be verified independently by customers through qualified professionals. Reference to brand names of other companies is for identification purposes only and does not imply recommendation or exclusion of similar available products.