PRODUCTS
Alkylsilane
Isooctyl Triethoxysilane
video
Isooctyl Triethoxysilane

Isooctyl Triethoxysilane

Product code: EB-538

CAS NO.: 35435-21-3

Molecular Formula: C14H32O3Si

Description: Isooctyl triethoxysilane is an organic silane impregnation material used for enhancing the durability of concrete, typically available in paste or liquid form. Primarily applied for the long-term protection of concrete structures, it possesses hydrophobic and waterproof characteristics. By penetrati

Products Description

Isooctyl triethoxysilane is an organic silane impregnation material used for enhancing the durability of concrete, typically available in paste or liquid form. Primarily applied for the long-term protection of concrete structures, it possesses hydrophobic and waterproof characteristics. By penetrating into the concrete substrate to a depth of 2–10 mm, it undergoes hydrolysis and condensation reactions to form a network-like hydrophobic membrane. This significantly improves the concrete's water resistance and resistance to chloride ion penetration. Its molecular formula is C₁₄H₃₂O₃Si.

Basic Information:

● 

Chemical Name: Triethoxy-(2,4,4-trimethylpentyl)silane

●  Alternative Name: Isooctyl Triethoxysilane

● CAS Number: 35435-21-3

● EINECS Number: 252-558-1

Molecular Weight: 276.4876

Molecular Formula: C₁₄H₃₂O₃Si

Chemical Structure:

Isooctyl Triethoxysilane

Physical Properties:

● Density: 0.878 g/cm³

● Boiling Point: 215.8 °C

● Flash Point: 95.9 °C

● Appearance: Colorless and transparent liquid

● Purity: ≥98%

Applications:

Isooctyl triethoxysilane is widely used across various industries, including paints, coatings, additives, wetting agents, electrical insulation, rubber synthesis, organic coatings, construction materials, and water treatment agents.

Notably, it is also employed in the corrosion protection of concrete structures. It effectively prevents deterioration caused by water ingress, sunlight, acid rain, and seawater, which can lead to corrosion, loosening, spalling, and mold growth in concrete and its embedded steel reinforcement. This significantly extends the service life of buildings.

Additionally, isooctyl triethoxysilane can be used in the production of specialized coatings to improve freeze-thaw resistance, reduce beading (anti-globulization), and minimize fine particle formation.

Packaging and Storage:

● Packaging: 180 kg per drum.

● Storage Conditions and Shelf Life: Store in a well-ventilated, cool, and dry indoor environment, away from direct sunlight.

Disclaimer:

All product information and technical recommendations provided herein are based on our current experience and level of knowledge. We assume no legal liability, including with regard to any third-party intellectual property rights that may be involved. No warranties or guarantees, either expressed or implied, are given regarding the properties of the product, especially in a legal sense. We reserve the right to modify product information at any time due to technological advancements or further developments. Customers are responsible for conducting thorough testing and evaluation of the product on their own. The descriptions of product properties in this document should be verified independently by qualified professionals. References to trademarks or brand names from other companies are for informational purposes only and do not constitute endorsement or exclusion of alternative or similar products.